This paper introduces a method of producing metallization pellet with laterite nickel ore as raw material and coal as a reductant in car bottom continuous furnace.
介绍了一种利用台车连续炉,以红土镍矿为原料,煤粉为还原剂,生产镍铁金属化球团的方法。
Thus, the proper basicity of Nickel oxide ore pellet is 1.10 in this experiment.
因此,本次氧化镍矿球团试验确定的合适球团碱度为1.10。